Chemical composition of Alloy P2000
C
|
Mn
|
Cr
|
N
|
≤ 0.15
|
% 12.0-16.0
|
% 16.0-20.0
|
% 0.75-1.00
|
Mo
|
Nb
|
Fe
|
Ni
|
% 2.5-4.2
|
≤ 0.25
|
rest
|
nickel free
|
Mechanical properties of Alloy P2000
solution heat treated
|
typical values
|
tensile s Rm
|
980-1120 MPa
|
yield strength Rp 0,2
|
610-720 MPa
|
elongation after fracture
|
55-65 %
|
reduction of area A
|
65-75 %
|
cold worked precipitation hardened
|
typical values
|
tensile strength Rm
|
over 2000 MPa possible
|
dimensions (Ø) mm
|
for samples only
|
0.8
|
●
|
1.02
|
●
|
1.30
|
●
|
Material Outlet by Hempel